GUIDE · TROUBLESHOOTING
Ten print failures and how to fix them
Most failed prints are one of ten problems. Changing five settings at once hides the cause; change one thing, then reprint a small test.
Check these three first
- Is the filament dry? Wet filament mimics a dozen other faults.
- Is the first layer right? Bed distance and cleanliness cause most failures.
- Did the slicer profile match the material? A PLA profile on PETG fails predictably.
1. Lifted corners — warping
Symptom: corners curl off the bed.
Cause: uneven cooling, draughts, low bed temperature, large flat area.
Fix: raise bed temperature slightly, add a brim, close the room, reduce part cooling on the first layers.
2. First layer not sticking
Cause: nozzle too high, oily bed, wrong bed surface, first layer too fast.
Fix: clean with dish soap, re-level, slow the first layer to 20 mm/s.
3. Stringing between parts
Cause: wet filament, too high nozzle temperature, insufficient retraction.
Fix: dry the spool first, then lower temperature by 5°C steps, then tune retraction.
4. Layer shift
Cause: loose belts, a nozzle catching curled edges, too much speed.
Fix: tension belts, enable Z-hop, reduce infill-to-wall overlap.
5. Extrusion stops — clog
Cause: heat creep, debris, wrong retraction distance, grinding extruder.
Fix: cold pull, check the hotend fan, cut a clean filament end.
6. Under-extrusion — gaps and weak walls
Cause: partial clog, low flow, slipping extruder, wrong filament diameter.
Fix: calibrate E-steps and flow, inspect the extruder gear for plastic dust.
7. Blobs and zits — over-extrusion
Cause: flow too high, moisture, seam placement.
Fix: lower flow 2–3%, dry filament, move the seam to a hidden edge.
8. Sagging overhangs and bridges
Cause: insufficient cooling, too fast, too hot.
Fix: increase part cooling, lower temperature, add supports where angles exceed 50°.
9. Split layers
Cause: low temperature, poor layer adhesion, high speed, wet material.
Fix: raise nozzle temperature 5°C, reduce fan, slow down.
10. Ringing — ripples on the surface
Cause: loose belts, high acceleration, heavy direct-drive head.
Fix: tighten belts, lower acceleration and jerk, check for frame wobble.
Summary table
| Symptom | Check first | Then |
|---|---|---|
| Warping | Bed temperature | Brim, draughts |
| No first layer | Bed distance | Clean bed, slow first layer |
| Stringing | Filament moisture | Temperature, retraction |
| Layer shift | Belt tension | Z-hop, speed |
| Clog | Cold pull | Heat creep, fan |
| Under-extrusion | Flow / E-steps | Extruder gear |
| Over-extrusion | Flow | Moisture, seam |
| Sagging | Cooling | Temperature, supports |
| Split layers | Temperature | Fan, speed |
| Ringing | Belts | Acceleration |
Safety
Do not reach into a moving machine. Let the hotend cool before removing a clog, and keep the printer on a surface that cannot tip.
Sources
Read next
Storing and drying filament