GUIDE · MATERIAL

Storing and drying filament

· Print Hub

Filament absorbs water from the air. At first nothing changes, then stringing gets worse and layers weaken. Most people notice only when settings that used to work stop working.

Temperatures below are ranges commonly published by manufacturers. The spool label and the manufacturer's instructions take priority.

Diagram of sealing, silica gel and a hygrometer
Three things are enough: seal, silica, hygrometer. Made by Print Hub.

1. Symptoms of wet filament

2. Some materials absorb faster

MaterialMoisture uptakeStorage
Nylon (PA), PVAVery fastSeal and dry immediately after opening
TPUFastDry before use
PETGModerateSeal for long storage
PLASlowSealing is usually enough
ABS / ASALowRelatively tolerant

PLA is not immune — it is just slower. Months in open air will affect it too.

3. Three storage rules

① Seal it. A zip bag or airtight box, spool and all. Store upright, away from sunlight and heaters — UV and heat deform plastic.

② Silica gel. One pack per container. Colour-indicating beads make replacement obvious. Wet silica stops absorbing and starts releasing, so it has to be regenerated.

③ Hygrometer. Put a small one inside the box. Aim for 10–20% RH; above 30% means replace or dry the silica.

4. Drying

A dedicated filament dryer is the safest option. Kitchen ovens vary too much and carry smell, contamination and fire risk. If you use one anyway, verify the real temperature with a separate thermometer and leave the door slightly open.

MaterialTemperatureTime
PLA40–50°C4–6 h
PETG55–65°C4–6 h
TPU50–60°C4–8 h
ABS / ASA65–75°C4–6 h
Nylon (PA)70–80°C6–12 h

Above the glass transition temperature a spool can deform. Never dry PLA at 70°C.

5. Common mistakes

Summary

Seal, dry, measure. Three habits remove most "my printer suddenly got worse" problems — and they cost less than a new hotend.